Looking for Help ?
Guides and technical data for every step, from degreasing to measurement.
Popular:
Where are you in the process?
Something went wrong?
Bubbles or voids in the replicaInject from the bottom up and keep the nozzle tip in the material.
Impression tore during extractionPull straight out. Never rotate it as if unscrewing a part.
Surface did not cure or stays stickyDegrease with DN1 first. Oil or residues block the reaction.
Curing is too slow or too fastPolymerization time depends on temperature. 20°C is ideal.
Marbled mix at the nozzle outletSet aside the non-homogeneous part until the mix is uniform.
Still need help? Talk to the Rivelec technical team
Ask a questionAtypical geometry or material. Describe your part, we recommend a procedure.Contact usBook a demoSee an impression taken and measured live on a video call.Pick a slot
Train your teamOur experts can come and meet your team to teach them how to use Plastiform in your very own process.Coming soon